The cooling system used in the screw is oil cooling, the cooling system used in the barrel is air-cooled, and all the screws are machined with high precision special CNC screw milling machine to ensure the same height of each similar extrusion equipment. Drawing on the current advanced design concept, the design concept of variable pitch, variable clearance and fine fluid mechanics calculation is adopted to make the material cut, kneaded and compacted more compactly and closer to the actual production Need.
1 Specification
Φ65/2~Φ150/2
Aspect ratio:16-35
Screw compression ratio can be based on different products and different formulations to design
2 Substrate material
1) 38CrMoAlA(JIS SACM645)
2) 42CrMo(AISI 4140)
3) 4Cr5MoSi V1 (JIS SKD-61)
3 Treatment Process
Quenched and tempered, qualitative, nitriding treatment.
4 Technical Parameters
Nitriding depth: 0.50mm-0.80mm
Nitriding hardness: 850-1000HV
Nitriding brittle: ≤level 1
Surface roughness: Ra 0.4
Screw straightness: 0.015mm